What E1 and E2 housings are
E1 and E2 are informal names for two sizes of low-profile power module with no copper baseplate and press-fit pins. The ceramic substrate that carries the dies forms the underside of the module and sits on the heatsink through a thin thermal interface layer; the PCB is pressed onto the pins from above, and screws through the plastic frame clamp the module to the heatsink. Makers sell these housings under their own names. One maker's mounting guide calls the two sizes F1 and F2 [1].
Without a baseplate the heatsink takes over the job of spreading heat, which a baseplate does somewhat better for short pulses, and the clamping force has to reach the substrate through the housing instead of through a stiff plate. The thermal performance of a baseplate-less module therefore depends strongly on the thermal interface material and on how evenly the housing presses the substrate onto the heatsink [6].
Press-fit or solder
A press-fit pin has a compliant zone, usually an eye-of-the-needle shape, that deforms as it is pressed into a plated through-hole and forms a gas-tight contact without solder. The technique dates from the early 1970s and is standardised in IEC 60352-5 [2]. For a power module it removes the solder step and the heat it puts into the module and board, and it allows a module to be pressed out and replaced [2].
Press-fit moves the requirements to the PCB:
- Board thickness of at least 1.6 mm, and a finished-hole diameter inside the tolerance the module maker gives for its pin [1] [2].
- A suitable plating finish. Hot-air levelled (HAL) plating is not recommended [1]; with ENIG, one maker measured lower press-out forces and does not allow the board to be reused after a module is pressed out [2].
- At least 4 mm between the centre of a press-fit hole and the edge of nearby components, so that the press tool can support the board and ceramic capacitors are not cracked [1] [2].
- A controlled press-in: one guide gives a speed of 25–50 mm/min following IEC 60352-5, a force of 40–80 N per pin, and a distance keeper on the tool to stop at the right depth [1].
Rework is limited. After a press-out the press-fit zone stays deformed. One maker allows a board to be reused once with a new module [1], another up to three times [2].
Thermal interface: pre-applied or your own
The thermal interface can contribute up to 60 % of the total thermal resistance between the dies and the heatsink, so it is the layer most worth controlling [3]. Many press-fit modules are offered with a phase-change material printed onto the substrate at the factory in a honeycomb pattern of fixed thickness. This removes the paste-printing step, and its variation, from your line [3].
Phase-change material is solid and wax-like at room temperature and softens above its phase-change point, about 45 °C for one common material; it reaches its intended thermal resistance only after it has flowed once [3]. One maker recommends 80 °C for 20 minutes for best spreading and notes that thermal impedance stays higher until the layer has melted, while another asks for the material to reach 60 °C once after assembly [1] [3]. The printed layer also gets thinner: in one guide a 160 µm layer on an F2-size module ends at about 86 µm after spreading [1].
Pre-applied material has a shelf life. One maker specifies storage at 5–40 °C and 10–65 % relative humidity for at most 24 months, after which the material is removed and replaced with grease [3]. If you apply your own grease, a guide for this package size gives 80–180 µm, a heatsink flatness of 50 µm per 100 mm or better and a roughness Rz of 10 µm or less [1].
Clamping and mounting sequence
The clamp screws set the pressure on the substrate. One guide specifies M4 screws with washers at 1.6–2.0 N·m, tightened either both at once or one after the other in a fixed sequence so that the module does not tilt [1]. Its order is: press the module into the PCB, apply or check the thermal interface, place module and PCB on the heatsink and tighten the clamp screws, then fix the PCB to spacer posts [1]. The posts sit at least 10 mm from the module edge and match the module height closely, so the board is not bent and the pins are not loaded; with several modules on one PCB, the guide adds posts between them [1].
Comparing on-resistance and current ratings
Check the conditions behind each number before comparing two datasheets.
- RDS(on) is usually quoted as a typical value at 25 °C and a stated gate voltage. For loss and thermal calculations the relevant value is the one at maximum junction temperature, which is also what the current-rating calculation uses [4].
- Continuous drain current is calculated, not measured: ID = √[ΔT / (Rth × R)], where ΔT = Tvj(max) − Tref, R is RDS(on) at Tvj(max), and Tref is the case or heatsink reference temperature [4]. A rating at a 25 °C reference assumes the reference can be held at 25 °C indefinitely, which no real heatsink does [4].
- Because the current scales with the square root of the temperature difference, the reference temperature alone moves the number. With Tvj(max) = 175 °C, a module rated at a 25 °C reference is rated about 80 % as high at an 80 °C reference, since √(95/150) ≈ 0.80 by the same formula [4].
- For baseplate-less modules the reference is often the heatsink, so the thermal resistance includes an assumed interface layer. Since that layer can be most of the total [3], compare junction-to-heatsink figures only for the same interface material and thickness.
- Some ratings are set by the terminals or pins rather than the dies. A terminal-limited figure does not grow with a better heatsink.
Paralleling modules
For more current, E2 modules are often connected in parallel. Static current sharing is set by differences in on-resistance, dynamic sharing during switching by differences in threshold voltage, and a mismatch in switching-loop stray inductance can also unbalance the on-state current with an inductive load [5]. The same work found coupling between paralleled dies inside one multichip module and showed that a substrate layout with an auxiliary source connection reduces it [5]. Imbalance means the combined rating is usually derated [5]. In practice: symmetric busbars, a gate resistor per module, a Kelvin-source gate return, one heatsink for all modules, and a derating agreed with the device maker.
Checklist
- Housing size, pin pattern and module height against your PCB and press tool [1].
- PCB thickness, finish and hole tolerance per the maker's press-fit specification [1] [2].
- Pre-applied or own thermal interface, its storage limit, and the first-heating step in your production flow [3].
- Screw size, torque and tightening sequence, and spacer posts for the PCB [1].
- RDS(on) at maximum junction temperature, and current ratings converted to your own heatsink temperature [4].
- On-resistance and threshold-voltage spread, and busbar symmetry, if you parallel modules [5].
Figures are from the cited sources, not from IRONHAWK measurements. IRONHAWK E2 press-fit modules are listed below; each part page gives its ratings and their conditions.
Related IRONHAWK parts
- IHSM23R005P2: 2300 V, 5 mΩ, E2 press-fit half-bridge SiC module
- IHSM12R004P2: 1200 V, 4 mΩ, E2 press-fit half-bridge SiC module
- IHSM12R006P2: 1200 V, 6 mΩ, E2 press-fit half-bridge SiC module
- IHSM12R008P2: 1200 V, 8.1 mΩ, E2 press-fit half-bridge SiC module
- HAWKPACK PF2: all E2 press-fit parts
Sources
- onsemi, AND90206/D “Mounting Guideline for F1/F2 Full Plastic Case Modules with Press-fit Pins”, application note, rev. 3, 2025. www.onsemi.com
- Vincotech, “Press-fit technology”, application note, rev. 05, 2012. a.storyblok.com
- Infineon, AN-2025-03 “Pre-Applied phase change Thermal Interface Material 2.0”, application note, rev. 1.1, 2026. www.infineon.com
- Texas Instruments, SLUAAT8, application note on MOSFET continuous and peak drain-current capability from thermal impedance, 2023. www.ti.com
- “Influences of Device and Circuit Mismatches on Paralleling Silicon Carbide MOSFETs”, IEEE Transactions on Power Electronics, vol. 31, no. 1, 2016 (Aalborg University; author version). vbn.aau.dk
- “Baseplate-less Power Modules Offer Thermal Resistance and Robustness”, EEPower, February 2024. eepower.com